Effect of glass fiber loading and reprocessing cycles on the mechanical, thermal, and morphological properties of isotactic polypropylene composites

In this study, a preliminary finding is carried out to obtain the optimum E-glass fiber content in polypropylene (PP) plastic products using loadings of 5, 10, 20, 30, and 40 wt%. The formulation with the optimum loading of 10 wt% glass fiber was reprocessed 10 times via extrusion and compression mo...