XRD, conductivity and FTIR studies on LiI-Li2WO 4-Li3PO4 prepared by low temperature sintering

Different amounts of Li3PO4 were mixed to a fixed ratio of LiI:Li2WO4, ground and pelletised before subjected to sintering at 70°C for 7 days. XRD shows that the product formed after sintering process is most likely Li6P4W 8O32 due to peaks present at 10.6°, 22.4°, 24.0°, 24.4, 26.2°, 32.4° and 34.0...